Causes and solutions for large pressure drop of brazed plate heat exchanger

Causes of large pressure drop in plate heat exchangers
1. the operating system pipeline is not properly purged, especially in the new installation system pipeline, many dirt (such as welding slag) into the interior of the plate heat exchanger, due to the plate heat exchanger The cross-sectional area of ??the flow channel is narrow, and the sediment and suspended matter in the heat exchanger gather in the corner hole and the flow guiding area, so that the flow channel area at the place is greatly reduced, and the pressure is mainly lost in this part.
2, after the plate heat exchanger has been running for a period of time, the pressure drop caused by the surface fouling of the plate is too large.
3. when the plate heat exchanger is selected for the first time, the area is too small, causing the flow rate between the plates to be too high and the pressure drop to be too large.
Processing method for large pressure drop of plate heat exchanger
1. remove dirt or plate fouling in the heat exchanger flow channel, for the newly run system, clean once a week according to the actual situation. When cleaning the surface scale of the plate (mainly CaCO3), use a 0.3 sulfamic acid solution or a 0.8 nitric acid solution containing 0.3 urotropin, 0.2 aniline, 0.1 potassium thiocyanate as the cleaning solution, and the cleaning temperature is 40-60 °C. When disassembling the equipment for chemical immersion cleaning, open the heat exchanger inlet and outlet of the heat exchanger, or install the DN25 cleaning port on the medium inlet and outlet nozzles when installing the equipment, inject the prepared cleaning liquid into the equipment, and wash it with water after immersion. Clean the residual acid to make pH≥7. When disassembling the cleaning, soak the plate in the cleaning solution for 30 minutes, then use a soft brush to lightly scale the scale, then rinse it with water. Avoid damage to the plates and rubber pads during the cleaning process. If the mechanical backwashing method is not disassembled, a nozzle shall be connected to the medium inlet and outlet pipes in advance, and the equipment shall be connected to the mechanical cleaning vehicle, and the cleaning liquid shall be injected into the equipment in the opposite direction of the medium flow, and the circulation cleaning time is 10 to 15 minutes. The medium flow rate is controlled at 0.05 to 0.15 m/s. After that, it is recycled several times with clean water to control the mass concentration of Cl in the water below 25 mg/I.
2. secondary circulating water is good to use soft water after softening treatment, generally requires the concentration of suspended solids in water is not more than 5mg / L, impurity diameter is not more than 3mm, pH & ge; When the water temperature is not more than 95 °C, the concentration of Ca and Mg should be no more than 2mmol/L; when the water temperature is greater than 95°C, the concentration of Ca and Mg should be no more than 0.3mmol/L, and the concentration of dissolved oxygen should be no more than 0.1mg/L.
3. for the central heating system, you can use a secondary water supply method.
2019/05/11 09:48:47 3738 Click

“十五五”启航 擘画保险蓝图——“2025年度中国保险鼎峰50人论坛”成功举办 贵州银行两名独立董事、一名董事、一名副行长任职资格获核准 华泰策略:A股春季行情的可能节点和潜在催化|华泰汽车 俞华军英大人寿董事、董事长的任职资格获批 杰瑞股份:公司燃气轮机发电机组成套设备应用领域广泛,包括石油天然气开发、数据中心、工业用电等|杰瑞股份 利用AI造谣“中国女篮” 两男子被刑拘 明年1月四成中日航线停售!被取消的运力转去哪里了|中国 视频|2分钟带您看懂一次性信用修复政策 香港创科局张曼莉:香港广纳人才布局 AI 生态圈,做好“超级联系人”“超级增值人” 云端进化,智启未来丨华为云数智领航会第四期圆满收官,共探AI场景落地|AI|华为云|智能化 AI是泡沫还是明天|AI 优刻得与比亚迪精密共建联合实验室|比亚迪 苏商银行黄金老:中国银行业应呈规模出海,寻求新的生存空间 特朗普五天圣诞长假期不会惠及大多数美国私企打工人 芳源股份:不存在逾期担保|证券日报 中国 REIT市场呈现高速扩容增长态势,开启房地产投资新赛道 关注俄乌冲突·美国国家情报总监发文称:北约和欧盟试图将美拖入与俄的直接对抗 湾区新引擎丨香港特区政府创新科技及工业局局长、驻粤办主任谈香港创科发展 晚间突发!创识科技实控人被立案并留置! 个人信用修复窗口限时打开,央行新政为非恶意失信群体重塑信用|信用 002175、600730,国资入局,下周一复牌!|方正